Industry News

Poor initial viscosity or non-stick

Update:23 Jan 2018
Summary:

Glue evaporation speed too fast or too slow --- adjust […]

Glue evaporation speed too fast or too slow --- adjust the rate of glue evaporation or change the construction process
Temperature is too low, affecting the initial viscosity --- adjust the temperature of the construction site or replace the low temperature glue
Gun air pipe water --- discharge air compressor water
Air temperature is too large --- adjust the construction site humidity environment
Sprayed adhesive layer is too thick, resulting in slow drying --- adjust the spray volume according to the correct method of operation
Spray coating is too thin, leading to fast drying --- adjust the spray volume according to the correct method of operation